PVC Paste Resin

General PVC Paste Resin GradeK value*Brookfield viscosityApplicationPF621633200Special PVC Paste Resin for foaming.PG680(68GP)683400Foam layer of synthetic leather, wallpaper, canvas, adhesive.PG740(74GP)742900Synthetic leather surfaces, canvas, adhesives, screen coatings, trademarks, toys, metal dipping, floor…

Continue ReadingPVC Paste Resin

Plasticizer

Eco-friendly Plasticizer Flame-resistant plasticizer Viscosity reducing plasticizer High and low temperature plasticizer Eco-friendly Plasticizer B-70:Fast gelation at low temperature. It is an Eco-friendly plasticizer, no separate out at high dosage.…

Continue ReadingPlasticizer

Dispersant

Q-300: dispersant Q-300 is a multifunctional liquid dispersant that can effectively disperse titanium dioxide, stone powder, carbon, AC foaming agent, etc.It is used in various PVC industries specially. After the…

Continue ReadingDispersant

Flame retardant

Antimony trioxide UltraCarb Triisopropylphenyl phosphate (phosphate ester flame-resistant plasticizer) Antimony trioxide General grade antimony trioxide (FR) Purity: ≧99.5% Average particle size: 0.6~1.2 μm Whiteness: ≧95 Lead content: ≦400 ppm Arsenic…

Continue ReadingFlame retardant

Lubricant

Grade Features and Applications RG-19 (liquid) Internal and external ester lubricant, with self-cleaning mold’s function, good mold releasing, contribute to processing stability. RG-60 (powder) Internal ester lubricant, application on rigid…

Continue ReadingLubricant