Grade | Features and Applications |
RG-19 (liquid) | Internal and external ester lubricant, with self-cleaning mold’s function, good mold releasing, contribute to processing stability. |
RG-60 (powder) | Internal ester lubricant, application on rigid PVC, semi-rigid PVC. It is beneficial for processing and appearance of product. |
RG-70 (powder) | Internal and external ester lubricant, it is beneficial for processing stability. It will not influence the penetrability. |
PE wax | WD2040PX | LP1020P | OX102P | LP0020P |
Brief | ‧ Thermal cracking | ‧ Refined PE homopolymer wax ‧ Derived from the ‧ Made in Thailand | .Low-density oxidized PE wax .Derived from .Made in Thailand | .Homopolyethylene wax .Derived from the .Made in Thailand |
Viscosity test method: ASTM D3236 | 350-450 cps (@ 140℃) | 10-20 cps (@ 149℃) | 200-300 cps (@ 140℃) | ≦ 20 cps (@ 149℃) |
Dropping Point test method: ASTM D3954 | 109℃ | 116℃ | 105℃ | 112℃ |
Acid Number test method: ASTM D1386 | – | 18 mg KOH/g | – | |
Certification | All comply with RoHS and REACH | |||
‧ Good compatibility with polyolefins ‧ Excellent pigment wetting ‧ Excellent lubricity (external lubricant, dispersant) ‧ Excellent chemical resistance ‧ Excellent thermal resistance and thermal stability ‧ Dispersants for carbon and fillers | ‧ High melting point and softening point ‧ low viscosity ‧ High heat resistance and stability ‧ High hardness standard ‧ Excellent chemical resistance ‧ Compatible with other waxes good compatibility ‧ Good slipperiness | ‧ Good slipping property ‧ Good compatibility ‧Good release properties ‧ Easy to emulsion ‧ Good transparency | ‧ High melting point and softening point ‧ Medium to low viscosity ‧ High heat resistance and high stability ‧ Excellent chemical resistance ‧ Compatible with other waxes ‧ Good compatibility slipperiness | |
Equivalent specifications | Clariant PE520 | Honeywell |